gotbots.si ← Volume 12 · Episode 3: Loose Corners The Enabling Layer · working papers
ELI G. · VOLUME 12 · EPISODE 3 · “LOOSE CORNERS”

Loose Corners: the fishbone & the defect data

First-pass yield on the door line sat in the high 80s — 88%, week after week — and nobody questioned it; it had become the plant’s normal. The crew had theories — handling, the press — but the plant ran its full Quality Systems instead: tally the defects, rank them, map the causes, and let the data settle the argument. It did. The trail ended at the PUR glue spreader.

Illustrative example: Eli G.’s plant is fictional. The data is synthetic, not a client case study.

4,000
Doors inspected
800 doors a day × 5 days — one production week
3,520
Passed first time
No repair, no rework
88.0%
First-pass yield
The same number week after week — treated as normal
480
Doors failed
Sent to the repair rack
600
Defect tallies
A failed door can carry more than one
70%
Loose veneer corners
420 of 600 tallies — the top defect
01

The board: 88% had become “normal”

Not a collapse — a constant. Week after week the board read 88%, give or take a point, and a number that never changes stops looking like a problem. That is how a chronic yield loss hides: not as an event, but as the plant’s normal.

First-pass yield — five weeks at the standing normal

Percent of doors passing inspection on the first pass, five straight weeks. Vertical axis runs 84–96%; each point is labeled with its value. There is no trend to read — the flat line in the high 80s is the story.

Why the flat line mattered

At 88%, 480 of 4,000 doors looped back for repair in a single week — and because it was 88% every week, the rack had come to look like a normal workstation instead of an exception.

The tally said the failures weren’t spread evenly across defect types. One defect — loose veneer corners — was doing most of the damage, and it was arriving already loose off the press. That pointed upstream, away from inspection and away from handling alone.

600 tallies across 480 failed doors = 1.25 defects per failed door, 0.15 defects per door inspected.

02

Defect data: tallies per door

The check sheet at final inspection counted every defect found, by type — not just pass/fail. A door with a loose corner and a scuff mark tallied twice, which is why 480 failed doors produced 600 tallies.

Pareto — defect tallies by type, one week (600 total)

Bars: tallies per defect type (left axis, from zero). Line: cumulative share of all tallies (right axis). Loose veneer corners alone are 70% — fix the corner and most of the week’s rework goes with it.

First-pass yield — high 80s, then a step change

Five baseline weeks in the high 80s — 88% was the plant’s unquestioned normal — then the two fixes land (new temperature controller, rollers on a definite change-out cycle) and yield steps straight to 99%. No slope: a step. Vertical axis starts at 80% and is labeled as such; every point carries its value. Part of the synthetic dataset built for Volume 12 · Episode 3.

The tally sheet, with per-door rates

Defect type Tallies Share % of tallies Cumulative Per 100 doors Per failed door
All defect types 600
100.0% 100.0% 15.00 1.25

“Per 100 doors” = tallies per 100 doors inspected (of 4,000). “Per failed door” = tallies per failed door (of 480). Synthetic dataset built for Volume 12 · Episode 3.

03

Fishbone: cause & effect

With the Pareto pointing at one defect, the team mapped every plausible cause of a loose veneer corner across the six classic categories — then tested them instead of voting on them. The Machine bone carried the answer.

EFFECT Loose veneer corners MACHINE ★ PUR glue spreader — confirmed Controller can’t hold PUR window Roller Teflon worn — coat drifts Rollers changed on failure only MATERIAL PUR adhesive behavior Viscosity swings with temp drift Thin passes starve edges first Corners get the least glue METHOD How the work was done Coat checks mid-panel only No temperature log per shift Weak bond found at handling MEASUREMENT What was never measured No weighed check at the edges Spreader temp never charted Tally never reviewed by defect type — 88% had become 'normal'. PEOPLE Handling & habits Handling finds weak corners Repair rack treated as normal Cause argued, not measured ENVIRONMENT Shop conditions Possible: shop temperature swings by shift Humidity shifts PUR cure Possible: cold mornings, worst counts

★ Confirmed by test: marked doors came out of the press with corners already light, and spreader temperature swung outside its window on the same shifts. Every other bone stayed a contributing condition — handling finds weak corners; it doesn’t make them.

Machine Root cause

  • Temperature controller couldn’t hold the PUR window — the spreader drifted hot and cold through the shift.
  • Roller Teflon surface deteriorating — as the coating wore, coat weight stopped being consistent across the sheet.
  • Rollers were changed when they failed, never on a schedule — so deterioration was discovered by defects, not by the calendar.

Material

  • PUR viscosity follows temperature: drift the temperature and the coat weight drifts with it.
  • On thin passes the edges and corners starve first — the middle of the panel still looks fine.
  • The bond at the corner was weak from the moment it left the spreader.

Method

  • Coat-weight checks were taken mid-panel, where the spread is most forgiving — never at the edges.
  • No temperature log per shift, so the drift left no trace until the defects did.
  • Nothing in the routine forced a look at the spreader — 88% was accepted as the line’s normal.

Measurement

  • No weighed coat-weight verification across the whole sheet — edges and corners included.
  • Spreader temperature was never put on a control chart; variation was invisible.
  • Tally never reviewed by defect type — 88% had become 'normal'.

People Contributing

  • Handling after the press flexes the corners — it reveals the weak bond, which is why it took the blame.
  • The repair rack had quietly become part of the process instead of a signal.
  • Two good theories (handling vs. the press) were argued hard — and settled only when the Quality Systems data came in.

Environment

  • Possible: shop temperature swings by shift add to the spreader’s own drift.
  • Humidity changes PUR cure behavior at the margins.
  • Possible: worst corner counts clustered on cold mornings — a clue that temperature, somewhere, was the story.

Root cause — confirmed

The PUR glue spreader couldn’t hold its process. Its temperature controller couldn’t hold the PUR window, so viscosity — and with it coat weight — swung through every shift; and its rollers’ Teflon surface was deteriorating, so even a good pass laid an uneven coat. Corners, which get the least glue to begin with, starved first. Everything downstream — the press, handling, the repair rack — was just meeting a defect that had already been made.

Fix 1 · Capital New temperature controller

Fitted to the spreader to hold the PUR window steady. Temperature is now logged every shift and charted — drift shows up on the chart before it shows up on doors.

Fix 2 · Discipline Rollers on a definite change-out cycle

Rollers are swapped on schedule, before the Teflon surface starts to deteriorate and take the coat weight with it — a calendar replacing a failure.

04

The toolkit in action

Volume 12 · Episode 3 wasn’t solved by one tool — it was the plant’s Quality Systems worked end to end, in story order. This is the Max Quality and VSM toolkit doing the job it exists for.

1

Check Sheet — the inspection tally

Every door inspected for a week; every defect marked by type at final inspection. 4,000 doors, 600 tallies. Without this sheet there is no episode — just opinions about yield.

2

Pareto — find the vital few

Ranked, the tallies speak plainly: loose veneer corners, 420 of 600 — 70%. Scuffs, cracks and machining preps share the rest. The investigation gets one target.

3

Fishbone — cause & effect

Every plausible cause of a loose corner mapped across Machine, Material, Method, Measurement, People and Environment — so the team tests causes instead of defending favorites.

4

5 Whys — down the Machine bone

Corner loose → bond starved at the edge → coat weight low on thin passes → viscosity drifting → spreader temperature out of its window → the controller couldn’t hold it. Five questions, one hardware answer — with worn roller Teflon compounding the coat-weight side.

5

Control Charts / SPC — temperature & coat weight

Spreader temperature and coat weight put on charts, shift by shift. The temperature trace swings beyond its limits on the same shifts the corner counts spike — variation made visible, and arguable no longer.

6

Process Capability — can the spreader hold spec?

The capability study answers the harder question: even on a good day, could this spreader — worn rollers, drifting control — hold coat weight at the edges? It could not. The process, not the people, was incapable.

7

FMEA — the loose-corner failure mode

The failure mode is scored for severity, occurrence and detection. Temperature drift and roller wear rank as the risks to engineer out — because inspection was catching the defect only after it had already tallied 420 times.

8

Standard Work + Control Plan — hold the fix

The countermeasures become routine: new temperature controller with per-shift temperature checks logged and charted; rollers on a definite change-out cycle, swapped before the Teflon deteriorates; weighed coat-weight checks across the whole sheet, edges and corners included.

9

A3 / 8D — the report-out

Problem, data, root cause, countermeasures and owners on one page for the plant: the high-80s yield board, the Pareto, the fishbone, the two fixes — and the control plan that keeps them honest.

10

Kaizen — lock the gains

A follow-up event watches first-pass yield recover and hunts the next defect on the Pareto — scuff marks now sit at the top of a much shorter list. The system keeps working after the episode ends.

11

Cost of Quality — price the failure

The rework loop is priced out in full — the repair cell’s labor plus the replacement veneer: $812,800 a year, about $15,631 a week, about $3.91 on every door. That is the number that turns a quality problem into a business case; the build-up is worked line by line in the Cost of Quality section below.

05

The value-stream view

Quality tools found the cause; the value-stream map shows what the defect was costing the flow. In the current state, about one door in eight takes a detour — that detour is pure waste.

Current state — door line with the rework loop

The rework loop (waste): 480 of 4,000 doors fail inspection → repair rack → re-inspection → back into flow. Every looped door is handled twice, waits twice, and carries the schedule with it — the Seven Wastes in one detour: rework, waiting, extra handling, and inventory stacked at the rack.

Future state — prevention at the spreader

The loop is designed out: control moves upstream to the spreader — temperature held, coat weight verified at the edges — so corners arrive at inspection already bonded. The repair rack goes back to being an exception, not a workstation.
06

Cost of Quality: the price of the loop

Failure has a payroll. The rework loop didn’t just slow the line — it carried a standing repair crew on every shift and a standing bill for replacement veneer. Priced out, the defect was one of the plant’s bigger cost lines.

The build-up — labor plus material

Cost line Basis Per year Per week Per door
Repair labor — the repair cell 4 people on each of 3 shifts — 12 people in total — at $40,000 a year each: 12 × $40,000 $480,000 $9,231 $2.31
Replacement veneer — rework material 2 in 3 reworked doors need new veneers on both sides — 2 veneers per door at $10 each. At the episode week’s rate — 480 reworked doors — that is 320 doors × 2 = 640 veneers a week: 640 × $10 = $6,400 a week $332,800 $6,400 $1.60
Total cost of quality Repair labor + replacement veneer $812,800 $15,631 $3.91

Per week = the annual figure ÷ 52 weeks (labor $9,231 + veneer $6,400 = $15,631, rounded). Per door = the annual figure ÷ 208,000 doors a year — 800 doors a day × 260 production days (labor $2.31 + veneer $1.60 = $3.91). The veneer line holds the episode week’s rework rate — 480 doors a week — across the year.

What the number says

The repair cell looked like capacity; on the books it was twelve people’s wages spent un-making a defect the spreader kept making — $480,000 a year before a single replacement veneer was counted. Add the material and the loop cost the plant $812,800 a year.

Spread across production, that is about $3.91 riding on every door the plant shipped — good doors included. That is the Cost of Quality argument in one line: the money for the new temperature controller and the roller change-out cycle was already being spent, every week, on repair instead.

07

The full toolkit: Max Quality & VSM

The same Quality Systems that found this root cause, all of it — every view in the plant’s Max Quality and VSM toolkit. The tools Volume 12 · Episode 3 actually used are marked.

Marked Ep. 3 = used in this episode’s investigation

The lesson of Volume 12 · Episode 3

A yield problem is never an inspection problem. The corner is where the process tells the truth: data over debate, a test over a theory, a root cause over a repair rack. One fix was capital — a controller. The other was pure discipline — a calendar. Both came out of the same toolkit.